Material: | stainless steel | Power: | 98% |
Method Used: | annealed | Frequency: | 35 kHz |
Depth: | <.001 | Speed: | 5 inches per second |
Laser Type: | 20 Watt Q-Switch Fiber Laser | Passes: | 1 |
Lens Focal Length: | 160mm | Cycle Time: | 5.8 seconds |
Sample was processed using a 20 watt Q-switched fiber laser through a 160mm F-theta lens.